It means, It is not correct to prepare a WPS supported my multiple PQR, with two condition, i.e. with PWHT and without PWHT. Also, instead of using two WPS on one joint, a new WPS is required to be prepared combining both WPS.
 
Please correct me if I am wrong.
 
Regards,
A, Husain

 
----- Forwarded Message -----
From: joseph mbé <mbejoseph@yahoo.fr>
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Sent: Monday, June 24, 2013 11:06 AM
Subject: Re: [MW:18018] WPS with multiple PQR

see my answer here below in red
 
Joseph Faustin Mbe
QA/QC Engineer
TEL CMR (00237) 33129846
TEL CG (00242) 057388009
BP 1155 Pointe Noire
Yesterday is the pass, tomorrow is the future; and today? Today is the present, the gift: Enjoy it!
 

De : Ahmed Husain <ahmraha@yahoo.com>
À : "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Envoyé le : Dimanche 23 juin 2013 17h00
Objet : [MW:18005] WPS with multiple PQR

Dear All, 
 
Followings are brief details of five PQRs.
PQR No.                 Process                       Base metal                             B.M. Thick      B.M. RANGE              PWHT                         Impact
 
#1                     SMAW                        P1Gr3 to P1Gr3                      0.24 Thk         1.6 -12                        N/A
#2                    SMAW                        P1GR3-P1GR2                        0.24 Thk          1.6 -12                         N/A                              YES (-51 F)
#3                    SMAW                        P1Gr3 to P1Gr3                      1.5 THK           16 - 200                       1150/10 HRS              YES (-51 F)
#4                    SMAW                        P1GR3-P1GR2                        1.5 THK           16 - 200                       1150/08 HRS               ES (-60 F)
#5                    SMAW                        P1Gr3 to P1Gr3                      1.75 THK         16 - 200                       N/A                              YES (-51 F)
 
 
Based on above PQRs,
 
1.    Is it acceptable to prepare  a single  WPS with two welding condition ( with and without PWHT), with notes stating thickness limits for both conditions. (why not 2 different wps )
2.    If yes, what would be thickness range for welding with & without PWHT. (PWHT is an EV so, not possible for my knowledge)
3.    With reference to ASME IX- QW-200.4 Combination of Welding Procedures,: If a company has two WPS, one in GTAW process and second in SMAW process, is it acceptable to apply individually both WPS on single joint? Or new WPS will be required combing both WPS? (Are you talking about 02 PQR or 2 WPS? if 02 PQR, Yes it's possible to use the combination of 02 PQR qualified separately but, in the limite of tickness range for each process). 
 
 
 Your valuable feedback will be highly appreciated.
 
Regards,
A.Husain
 


The contents of this email, including all related responses, files and attachments transmitted with it (collectively referred to as "this Email"), are intended solely for the use of the individual/entity to whom/which they are addressed, and may contain confidential and/or legally privileged information. This Email may not be disclosed or forwarded to anyone else without authorization from the originator of this Email. If you have received this Email in error, please notify the sender immediately and delete all copies from your system. Please note that the views or opinions presented in this Email are those of the author and may not necessarily represent those of Saudi Aramco. The recipient should check this Email and any attachments for the presence of any viruses. Saudi Aramco accepts no liability for any damage caused by any virus/error transmitted by this Email.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 


Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...