Re: [MW:17598] Regarding Kereosene Leak test

dear Balaji 

Kerosene Test is one type to find out  leakage on root . to Perform kerosene test u need to Spray Kerosene on Root Surface. from on side of joint. and other side you need to apply white chock or  white powder .

once Spray , Kerosene . Wait Up to 30 Minutes Minimum. and Check other side white Surface .
if any Kerosene ,Marks if you seen on white Surface ,then we can consider as Defective Area.


Regards 

Ritesh Rajput 



On Tue, Apr 30, 2013 at 4:49 PM, balaji s <borntowin2k12@gmail.com> wrote:
Dear Experts,
 
Here our contractor fabricated the ducts for FDA.
 
To examine the weld quality Kerosene leak test to be done.
 
1.Anybody having the procedure for Kerosene Leak test.
 
2.For duct welding other than Kerosene test is available?
 
Please Suggest me.
 
Regards,
Balaji

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

[MW:35738] ASME IX WPS Qualification Query: GTAW + FCAW with Multiple PQRs

Dear Welding Experts, I'm currently preparing a Welding Procedure Specification (WPS) and have encountered a request to qualify a GTAW +...