Dear experts,

 

Kindly explain following queries

(a)   PWHT holding time for P91 mentioned in B 31.1 is 1 hr/25 mm; minimum 30 minutes. Does it mean that if the thickness is 6/10/12.5 mm the holding time is 30 minutes & for 15 ,20,30,40 mm the holding time is 36  48,72,96 minutes respectively.

(b)    I got some special heating curves for P 91 from our group. But Kindly explain about the reference /standard used for preparation of this heat curve ( eg- why the preheat maintenance is 4 hours & again free cooling).

I raised these doubts earlier in [MW:17585], but I didn’t receive any response. Please give your comments.

 

 

S.Binoy

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...