RE: [MW:16915] How filler wire & electrode selected for GTAW & SMAW

Dear Friend,

 

304L to 304L, ER 308L will be better than E 304L.

 

Thanks,

With kind regards,

M. Vedaraju

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of c sridhar
Sent: Friday, March 01, 2013 3:52 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:16907] How filler wire & electrode selected for GTAW & SMAW

 

Mr. Chandhra Sekar,

With ref. to your request,

                                                                                                    GTAW                    SMAW
1. A240 TYPE 304 TO A240 TYPE 304L                  use            ER 304L                E 304L
2. A240 TYPE 304 TO A240 TYPE 316L                  use            ER 316L                E 316L
3. A240 TYPE 316L TO A240 TYPE 316L                use            ER 316L                E 316L
4. A240 TYPE 321  TO A240 TYPE 304                   use            ER 321                  E 321

Sridhar.


From: chandra sekaran <chandrasekaran.vcs@gmail.com>
To: materials-welding@googlegroups.com
Sent: Monday, 25 February 2013 3:00 PM
Subject: [MW:16865] How filler wire & electrode selected for GTAW & SMAW


Dear Welding experts,

I like to know how we are selecting the filler wire and electrode for
Steel & Steel alloys.
Based on the tensile strength of the base material it is selected. I
need the specific technical parameters how we are selecting the filler
wire or electrode. Please guide me for the process,


GTAW                  SMAW
1. A240 TYPE 304 TO A240 TYPE 304L
2. A240 TYPE 304 TO A240 TYPE 316L
3. A240 TYPE 316L TO A240 TYPE 316L
4. A240 TYPE 321  TO A240 TYPE 304

Best regards,

V. Chandrasekaran

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.



--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...