Skip to main content

Re: [MW:16796] Re: Suitable Weld metal for P1 to P4 material

Once again, P1 will gouvern in the selection of the filler metal. the filler metal should be for the lower grade

Rgds.

 
Joseph Faustin Mbe
QA/QC Engineer
TEL CMR (00237) 33129846
TEL CG (00242) 057388009
BP 1155 Pointe Noire
Yesterday is the pass, tomorrow is the future; and today? Today is the present, the gift: Enjoy it!
 


De : Sivadas98 <sivadas98@gmail.com>
À : materials-welding@googlegroups.com
Envoyé le : Samedi 16 février 2013 10h34
Objet : [MW:16789] Re: Suitable Weld metal for P1 to P4 material

Dear Dharmadattu,

For selecting a electrode/filler metal for two dissimilar metal you have to choose the Electrode/filler metal of higher grade material.i.e if you want to weld P4 to P1 you have to select electrode of P4 material.
   

On Saturday, February 16, 2013 12:30:38 PM UTC+4, Dharma dattu wrote:
Dear Experts,
Thanks for the solution. But what is the method for  selecting electrode / filler metal for welding of two dissimilar metals
 
Regards,
 
Dharmadattu.B
On Friday, 15 February 2013 15:52:00 UTC+5:30, Dharma dattu wrote:
Dear Experts,
What is the method for  selecting electrode / filler metal for welding of two dissimilar metals. at present i need to establish a WPS for IS 2062 to SA 387 Gr.11 Class 2. Which are P1 & P4 materials respectively.

Regards,

Dharmadattu.B
Hyderabad

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 


Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...