[MW:16046] RE: welding with EL8

Hi Kiran,
 
For SAW the wire flux classification is important than filler metal alone. Sec-IX,QW-404.9 addresses this issue.
 
A change from EH14 (1.8% Mn) to EL8( less than 1% Mn) would cause significant reduction in weld metal mechanical properties.
 
Hence this change may not be allowed unless a new PQR is qualified.
 
Thanks.
 
 

Pradip Goswami,P.Eng.IWE

Welding & Metallurgical Specialist

Ontario, Canada.

Email-pgoswami@sympatico.ca,

pgoswami@quickclic.net

 


From: kiran kumar [mailto:chvvn.kirankumar@gmail.com]
Sent: Monday, November 26, 2012 3:54 AM
To: pgoswami@sympatico.ca; pgoswami@quickclic.net
Cc: materials-welding@googlegroups.com
Subject: welding with EL8

Dear Sir
 
Can we weld with Filler wire  EL8 with supporting PQR  EH 14 Filler wire (having same F no:6)
 Material IS 2062
 Construction code -BPVC Section IX
 Process-SAW Process.
 
Thanking you
 
CH.V.V.N.KIRANKUMAR
 