Skip to main content

RE: [MW:15371] Re: Socket weld gap requirement

Hi Naresh,

Please see the interpretation of ASME on requirements of gap for socket welds and the NDE following welding . The prime function of this gap is to facilitate the expansion and contraction of the thinner components in the  socket weld fit-up, especially the piping.

This gap is required during the fit-up , not after welding. In your case(as mentioned below) there should not be any violation of code approved practice.

Thanks.


Pradip Goswami,P.Eng.IWE
Welding & Metallurgical Specialist
Ontario, Canada.
Email-pgoswami@sympatico.ca,
pgoswami@quickclic.net

Interpretation: 19-5-
http://cstools.asme.org/csconnect/pdf/CommitteeFiles/23730.PDF


-----Original Message-----
From: materials-welding@googlegroups.com [
mailto:materials-welding@googlegroups.com] On Behalf Of ranendrac6@gmail.com
Sent: Sunday, September 23, 2012 11:25 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:15370] Re: Socket weld gap requirement

The gap is required to release the fume gases which generated during welding. No gap required after welding(I don't see any reason).  You can check with 4 mm gap during fit up to meet client requirement.
Sent on my BlackBerry® from Vodafone

-----Original Message-----
From: Raghuram Bathula <raghurambathula@gmail.com>
Sender: materials-welding@googlegroups.com
Date: Sun, 23 Sep 2012 08:10:03
To: Materials & Welding<materials-welding@googlegroups.com>
Reply-To: materials-welding@googlegroups.com
Subject: [MW:15368] Re: Socket weld gap requirement

no it it not required after welding, many times gap closes to zero due to shrinkage during welding. if your client requires the gap after welding (I don't see any reason for this) probably you need fit up with more gap.

On Sep 22, 7:49 pm, Naresh Kumar <snareshkuma...@yahoo.com> wrote:
> Dear experts,
>
> As per ASME 3.1.& 31.3 socket weld gap requirement is 1/16” before
> welding. Whether it is required for after welding, if its require
> kindly provide the code details.In our project we're done RT for
> socket welds. But after welding did not find the 1/16” gap, its less
> than 0.5mm.
Our client decision is to cut and reweld the all joints.
>
>
> Thanks & Regards,
> Naresh

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...