If PWHT is process requirement (Sau caustic) then any repair on job after PWHT calls for re-PWHT(Of course you need to qualify welding procedure also)
However if PWHT requirement is due to base metal thk then depends if repair depth  after PWHT is less than thk that require PWHT as per code then i feel PWHT may not be required(But u need to qualify the welding procedure for this also)

Regards
Sachin.Sankhe

From: Dindo <dindodelacruz@gmail.com>
Sent: Sat, 15 Sep 2012 21:18:29
To: materials-welding@googlegroups.com
Subject: Re: [MW:15304] Repair after PWHT - B 31.1
First thing is you have to do your due dilligence by doing NDT prior to sending for PWHT, so that you wont get caught unaware of the repair before it goes to the oven.
 
Second thing is if there is a repair after PWHT, then you have to cut out the whole weld and redo the weld.
 


 
On Wed, Sep 12, 2012 at 10:17 PM, hemant <hsuthar@chemithon.co.in> wrote:

Dear Jignesh Sir,

As per metallurgy point of view we can done PWHT cycle only one time if we go for second time we have to qualify Repair WPS.  Pls reply me for any suggestion.

 

Thanks,

HHS

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Desai Jignesh (Mumbai - Piping)
Sent: 12 September 2012 09:31
To: materials-welding@googlegroups.com
Subject: RE: [MW:15276] Repair after PWHT - B 31.1

 

I would like to highlight requirement out lined in ASME B 31.3 as below.

 

# Refer Para 341.3.1(a)

 "For P-Nos. 3, 4, and 5 materials, examination shall be performed after completion of any heat treatment"

 

# Refer Note (11) in "NOTES FOR APPENDIX A TABLES " (Pg 147 – 2010 edition)

"For use under this Code, radiography shall be performed after heat treatment"

This note(11) pointing P3, P4, P5A, P5B, P9A & P9B materials only as per table A-1.

 

And of course, Re-PWHT shall be carried out if any repair comes, in case of RT after PWHT.

 

Regds/Jignesh

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Siva
Sent: 11 September 2012 12:19
To: materials-welding@googlegroups.com
Subject: Re: [MW:15269] Repair after PWHT - B 31.1

 

PWHT shall be done after weld repair. So my understanding is, to find weld repairs, we need to perform NDT before PWHT. I have seen in my experience, normally, NDT will be done prior to and after PWHT also(i.e., twice on that joint).
If NDT done only after PWHT, found any defects, then after weld repair, again should perform PWHT, which might effect mechanical properties.

On Mon, Sep 10, 2012 at 9:10 AM, sevak hiren <hirensevak80@gmail.com> wrote:

Dear Experts,

Piping Code : ASME B 31.1, Power Plant Piping, (P No.5A,11,12,15, 91 etc pipes) & ASME Sectin I

Contractor is doing piping fabrication stages in following manner,

Preheating & Welding of Piping joints then Post heating, then PWHT & then finally RT.

Contractor is arguing, RT is taken after PWHT  to reveal the defects causing due to delayed cracking.

My question

If RT repair is done for particular joint after PWHT then is it compulsory to perform PWHT again for particular joint ? if yes then please mention the clause of code.

Thanks & Regards

Hiren Sevak




--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 




--

Regards,
G.Sivalingam., BE.,
Quality Control Inspector - Welding,
SAS Project, Abu Dhabi, UAE.

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 


Follow Rediff Deal ho jaye! to get exciting offers in your city everyday.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

Comments

Popular posts from this blog

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

[MW:5202] RE: 5200] NDT after PWHT

------------------------------------- Interpretation:  I‑89‑14 Subject:         Section I (1986 Edition, 1987 Addenda), PW‑11,                  NDE Prior to PWHT Date Issued:     December 15, 1988 File:            BC88‑393   Question: Does PW‑11 require that NDE be performed on welds after they have been subjected to the postweld heat treatment required by PW‑39?   Reply: No, unless the conditions described in PW‑11.2.2 exist. ---------------------------------------------- Interpretation:  VIII-1-98-09 Subject:         Section VIII, Division 1 (1995 Edition, 1996 Addenda); NDE                 ...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...