Re: [MW:14710] GTAW wires equivalent to AWS E10018-D2 and E 11018M

Hi
 
You can use the following GTAW consumables ER 110S-G. In India you can use Bohler brand.
 
Regards
 
Prem Nautiyal
Cell: 9769316004

From: ARC WELDING COMPANY <arcweldingcom@gmail.com>
To: materials-welding@googlegroups.com
Cc: arcweldingcompany@gmail.com
Sent: Wednesday, June 27, 2012 10:56 AM
Subject: [MW:14702] GTAW wires equivalent to AWS E10018-D2 and E 11018M

Dear sir,
Can anybody suggest GTAW consumables equivalent to AWS E10018-D2 and E 11018M?
Thanks and regards,
For Arc Welding Company,
Anil Verma
9999200148
 
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...