Friday, April 13, 2012

[SUSPECTED SPAM] Re: [MW:14106] Hardness value without PWHT

----- Original Message -----


Dear friend,
First of all pl confirm which welding procedure you used (i.e.GTAW+SMAW),or any one?

See if you use welding technique GTAW by ER80SB2 + SMAW by E8018B2 hardness value will may be in controll.
Pl try & revert.

Regards,
RK Vichare


From: pradip kumar sil <pradipsil@gmail.com>
To: materials-welding@googlegroups.com
Cc: pgoswami <pgoswami@quickclic.net>
Sent: Thu, 12 Apr 2012 10:50:16 +0530 (IST)
Subject: [MW:14104] Hardness value without PWHT

Dear experts,
I have faced regarding hardness issue on ASTM A 335 GR P-11 material.
Pipe thickness is 7.5mm. Without PWHT hardness is coming around 275
to 289 BHN on weld zone & 250 260 BHN on HAZ zone & parent material
hardness is 197 to 204 BHN. Due to inside refractory material PWHT is
not possible.
My question is as per ASME B-31.3/ ASME SEC II PART A hardness value
of this material is 225 BHN ( MAX). There is any specification for
weld zone / HAZ zone hardness value.
Can anybody give an idea to reduce the hardness without PWHT if it is
not acceptable limit.
Thanx in advance.

Regards
Pradip

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...