Re: [MW:14162] Thickness range for radiography techniqu qualification

Dear Mr. Satish,
 
Please refer below extracts of UW-51 (a) of ASME Sec. VIII Div. 1

(2) A written radiographic examination procedure is

not required. Demonstration of density and penetrameter

image requirements on production or technique radiographs

shall be considered satisfactory evidence of compliance

with Article 2 of Section V.

 

Thanks & regards,

 

 

C. R. GANDHI
--- On Mon, 4/23/12, Satish Patel Manubhai <satish19183@yahoo.co.uk> wrote:


From: Satish Patel Manubhai <satish19183@yahoo.co.uk>
Subject: [MW:14139] Thickness range for radiography techniqu qualification
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Date: Monday, April 23, 2012, 2:21 PM

Dear all,
Good afternoon.
As per section V we have to go for procedure qualification before the start the radiography in job.
Is there any group range for dia and thickness for the procedure qualification or we have to go for all individual dia and thickness.
Kindly advise and also give reference code for the same.
Regards,
satish patel
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...