Wednesday, April 25, 2012

Re: [MW:14150] alignment tolerance

ASME Sec VIII Div 1 does not state tolerance on vessel straightness which is customer specific. However, most customers specify the straightnee as 1mm per meter with max limit of 19mm for vertical vessels.

Gopal
Sent from BlackBerry® on Airtel

From: prashant pansare <prashantpan_99@yahoo.co.in>
Sender: materials-welding@googlegroups.com
Date: Wed, 25 Apr 2012 20:30:53 +0800 (SGT)
To: <materials-welding@googlegroups.com>
ReplyTo: materials-welding@googlegroups.com
Subject: Re: [MW:14149] alignment tolerance

Dear Sir,
 
UW 33 describes about offset.
My rquirement is regarding alignment of shells.
For 60 Mtr. Long Column what is the alignment tolerance?
 
Regds,
PSP 

--- On Wed, 25/4/12, vincer michael <vincermichael@gmail.com> wrote:

From: vincer michael <vincermichael@gmail.com>
Subject: Re: [MW:14148] alignment tolerance
To: materials-welding@googlegroups.com
Date: Wednesday, 25 April, 2012, 10:15 AM

To See UW-33, AND TABLE UW-33

On Tue, Apr 24, 2012 at 7:58 PM, prashant pansare <prashantpan_99@yahoo.co.in> wrote:
Dear All,
 
what is the maximum alignment tolerance as per ASME Sec VIII Div 1?
 
Thanx
 
PSP
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Thanks
With Best Regards,
D.VINCER MICHAEL
+91-8264447884

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...