Tuesday, April 17, 2012

Re: [MW:14115] welding after hydrostaic test

Dear Himan
 
The code not clearly mentioned as what you need. But from my experiences, is not allow you to do weld repair after complete hydrostatic test. You can refer ASME VIII Div II clause 6.4.5.2. Weld repairs made after PWHT as reference.
 
Regards
Ghafor Mohamad
Welding Engineer 

On Mon, Apr 16, 2012 at 2:29 PM, Himan Nikdin <himannikdin@gmail.com> wrote:
Dear experts
 
I would appreciated if anyone can share some refrence (code) regarding allowance of welding after hydrostatic test on pressure vessle which repair area fully radiographed and the result is accepatble.
 
Regards,
himan Nikdin

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...