Martin,

I seems that you are welding Bisalloy 80. So, because of the risk of stress relieve cracking PWHT should not be undertaken unless it is absolutely necessary. However if it is really unavoidable, PWHT should not exceed the tempering temperature and  before stress relieve is applied, the toe of the weld should be blend by grinding in order to  minimise occurrence of stress relieve cracking.

 

Hope it helps

Ariel

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Martin Prad
Sent: Friday, 6 April 2012 6:52 PM
To: materials-welding@googlegroups.com
Subject: RE: [MW:14072] RE: 14069] PWHT of a seam welded with rutile wire

 

It is a low alloy medium tensile steel welded with E81T1 flux cored tubular wire. Can generally the weld seams welded with this type of wires be stress releived? Is the any unforeseen issues on behind of it?
 


From: ariel@iinet.net.au
To: materials-welding@googlegroups.com
Subject: [MW:14071] RE: 14069] PWHT of a seam welded with rutile wire
Date: Fri, 6 Apr 2012 15:36:43 +0800

Martin

Rutile flux is used to weld mild steel and is very ductile so no PWHT is usually required. In what type of wire was it in,  and what type of steel was it used on?

 

Ariel

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Martin Prad
Sent: Friday, 6 April 2012 2:02 PM
To: materials-welding@googlegroups.com
Subject: [MW:14069] PWHT of a seam welded with rutile wire

 

Friends,
 
Have you faced with any issues after PWHT of a weld seam welded with rutile type Flux Cored wedling wire?
 
regards,
Martin.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...