Thursday, April 5, 2012

Re: [MW:14066] suggest the welding procedure to weld WCB with SS 410 ring


Hi,

Use E309L electrode to avoid any PWHT.
Do some pre heating on P6, generally about 100 degree for 10mm thickness.

Regards,
Zakir Ali.
Sr. Manager - Welding.


From: vpuranik <vpuranik@deltechcontrols.com>
Sent: Wed, 04 Apr 2012 16:37:33
To: <materials-welding@googlegroups.com>
Cc: Mallikarjun Patil <m.patil@deltechcontrols.com>
Subject: [MW:14049] suggest the welding procedure to weld WCB with SS 410 ring

Dear experts,

 

Please suggest the welding procedure and welding parameters to weld WCB body and SS 410 Ring and also suggest welding electrode for welding.

 

 

Thanks & Regards.

 

Vaibhav V Puranik.

(Manufacturing Engineer)

 

Delval Flow Controls (P) Ltd.

Gat.No.625 /1/2,Kuruli,3

Tal Khed,Pune-Nashik Highway,

Pune-410501,India

Phone:02135-662700 / 662716.  Fax: 02135-662727

Cell:+91 8308829850 Email: vpuranik@deltechcontrols.com

I could not wait for success, so i went ahead without it.

Logo1

 

 

 

 

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


-----------------------------------------
Delval Flow Controls Pvt Ltd, Pune, India



Follow Rediff Deal ho jaye! to get exciting offers in your city everyday.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35738] ASME IX WPS Qualification Query: GTAW + FCAW with Multiple PQRs

Dear Welding Experts, I'm currently preparing a Welding Procedure Specification (WPS) and have encountered a request to qualify a GTAW +...