Sunday, April 29, 2012

[MW:14164] Inconel 625 overlay on AISI4130 material using SMAW process

Hi

I would be qualifying Inconel 625 overlay on AISI4130 material using SMAW process. Any precautions/ guidance in this regarding would be much appreciated