Sunday, April 22, 2012

[MW:14138] gaskets for 30% caustic concentration at 140 C Degree temp

Dear friends,

we use grafite with monel embeded gaskets for caustic 30% conc. at 140
C temperature lines, but frequently it leaks after few months in
service (max. 6months), after opening the flange joints we found the
gaskets were totally failed. The line material is Ni-200 with stub
ends and lap joint flanges.

Kindly suggest the appropriate gaskets to avoid frequent leakages from
flange joints.
(photos could not be attached due to lager sides)

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...