[MW:14103] Re: Max allowable offset

Please refer UW-33 clause b, the code itself permits any offset within
the allowable tolerance provided in table UW-33 shall be faired at a
three to one taper over the width of the finished weld. So u can taper
the ID when offset is morethan permitted in table UW-33.

Sandeep.
QC Engineer

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.