Friday, April 6, 2012

[MW:14071] RE: 14069] PWHT of a seam welded with rutile wire

Martin

Rutile flux is used to weld mild steel and is very ductile so no PWHT is usually required. In what type of wire was it in,  and what type of steel was it used on?

 

Ariel

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Martin Prad
Sent: Friday, 6 April 2012 2:02 PM
To: materials-welding@googlegroups.com
Subject: [MW:14069] PWHT of a seam welded with rutile wire

 

Friends,
 
Have you faced with any issues after PWHT of a weld seam welded with rutile type Flux Cored wedling wire?
 
regards,
Martin.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...