Thursday, April 12, 2012

Fwd: [MW:14105] Re: Regarding Electrode Weaving

As your weaving width increases there will be maximum chances of slag entrapment at both sides (left & right) because of prior solidification of weld before welding of respective edges. Your weld pool should be in fused state during weaving to avoid slag entrapment.

Regards,
Maulik
Welding Engineer
Larsen & Toubro

---------- Forwarded message ----------
From: Karthik <karthik6684@yahoo.com>
Date: Wed, Apr 11, 2012 at 9:38 AM
Subject: [MW:14091] Re: Regarding Electrode Weaving
To: Mohit Aggarwal <aggarwalmohit05@gmail.com>, "george.dilintas@gr.bureauveritas.com" <george.dilintas@gr.bureauveritas.com>, AA karandish <aa.karandish@yahoo.com>, Abuhanip bin Abdul <abuhanip@labuanship.com>, Ahmed Osman <a.osman81@yahoo.ca>, akcme <akhilcme@gmail.com>, Ali Asghari <asghariali@rocketmail.com>, Aly <mhaskar.aly@gmail.com>, AMIT PAHUJA <amitpahuja2@gmail.com>, Amos Majola <amos@turnmill.co.za>, Anil Hegde <nottyanil@gmail.com>, antony jenis <antonyjenis@gmail.com>, Arun Jacob <jacob.igcs@gmail.com>, Arunachalam A <arunvani@gmail.com>, Ary Agung Prasetyo <ary_mt05@yahoo.com>, asad azmi <azmiasadayub@gmail.com>, Brl Pp <refazosaris@gmail.com>, Dindo <dindodelacruz@gmail.com>, Dinesh Somwanshi <som.din@gmail.com>, duc hoang <hoangvanduc79@gmail.com>, ENAYAT ZAREI <zarei.enayat@gmail.com>, Endri Prasetyo <endri.prasetyo@gmail.com>, Fitria Rahman <t.chintaqa@gmail.com>, fredric <fredric.prabu@bwgindia.com>, "Garry Mat Eng." <garryirwin342@gmail.com>, Himan Nikdin <himannikdin@gmail.com>, james gerald <gerry_tup@yahoo.com>, John Henning <jhenning@deltak.com>, jose <joseseban@gmail.com>, Kaja Mohideen <kaja@asw.sa>, kannayeram gnanapandithan <kgpandithan@gmail.com>, Kavin Murugam <kavin202082@yahoo.com>, ketan shah <ai.ketan@gmail.com>, khemici badri <khemicib@yahoo.fr>, lakshman kumar <lakshmankumar4@gmail.com>, Madhusudan Rout <madhusudan.rout@gmail.com>, mahesh sanghvi <sls.mahesh@gmail.com>, Mahmoud <mqreis@gmail.com>, materials-welding <materials-welding@googlegroups.com>, meemo prasad <meemoprasad@gmail.com>, Mehdi Emami <mehdi.emami@yahoo.com>, mpk mpk <ranmi2007@gmail.com>, MRG <mrgupta_2007@yahoo.com>, muthu barathi <muthu_barathi@rediffmail.com>, "Nadgauda, Subhas" <subhas.nadgauda@jacobs.com>, Nandesh Kumar <nandeshkumar@rocketmail.com>, Narendra Gohil <ngohil@qafco.com.qa>, Neilash Kumar <neilashkumar@yahoo.com>, Nizam Mohamad <ahmad.nizam83@yahoo.com>, pgoswami <pgoswami@quickclic.net>, Pieper QSI <info@pieper-qsi.nl>, "prabhakarmet@gmail.com" <prabhakarmet@gmail.com>, prem nautiyal <prem_nautiyal26@yahoo.com>, "R.Lenin" <lenin8319@gmail.com>, rajeev arora <rajeevarora007@gmail.com>, rajkumarantoni <antonitr@gmail.com>, Ramchandra vichare <vicharerke@indiatimes.com>, Ramin Kondori <raminkondori@gmail.com>, ravi varman <ravimvarman@gmail.com>, S C Balawat <scb12345@gmail.com>, sanggyu LEE <sgleehong@gmail.com>, santhosh kumar <santhoshgu7@gmail.com>, SAQIB SHIRAZI <saqibshirazi83@hotmail.com>, sevak hiren <hirensevak80@gmail.com>, shanmuga mari <85.ssmari@gmail.com>, snbagchi <snbagchi@aol.in>, Srinivas Engr <srinivas.gmsrini@gmail.com>, srinivasu <srinivasu.mech@gmail.com>, "T. Mahendran" <cbemahendar@yahoo.com>, U WYNN-NAING <u.wynn-naing@total.com>, vaibhav Joshi <vnjoshi.leo@gmail.com>, venkat ramana <venkatgps.ramana@gmail.com>, Vijay Katkar <katkar.vijay22@gmail.com>, "vinit.deshpande" <vinit.deshpande@akersolutions.com>, Vino Varghese <vinopvarghese@gmail.com>, Wu Hua <jointstars@yahoo.com>, yogeshkumar Kumbhar <kumbharyogeshv@gmail.com>, ZUL MAS <zulmas77@yahoo.com>


Hi,
As per Code it is a Non essential variable and Code doesn't specify the weave bead width limits. But you have to specify on the WPS (Stringe/Weave bead). Its a good engineering practice to limit the weave bead width to control the heat input.
 
Thanks & Regards,

(Karthik)

Karthikeyan.S
QA/QC Manager
German-Thai Boiler Engineering Cooperation Limited.
Rayong Factory ;
379 Moo.6 Soi 8, Tambol Pananikom,
Nikompattana, Rayong 21180 THAILAND
Tel : +66 38 897 035-9 Ext. 137
Fax : +66 38 897 034
Hand Phone: 0066 892512282

From: Mohit Aggarwal <aggarwalmohit05@gmail.com>
To: christopher_rajku...@yahoo.com; george.dilintas@gr.bureauveritas.com; manojac...@gmail.com; welding_engr_r...@charter.net; AA karandish <aa.karandish@yahoo.com>; Abuhanip bin Abdul <abuhanip@labuanship.com>; Ahmed Osman <a.osman81@yahoo.ca>; akcme <akhilcme@gmail.com>; Ali Asghari <asghariali@rocketmail.com>; Aly <mhaskar.aly@gmail.com>; AMIT PAHUJA <amitpahuja2@gmail.com>; Amos Majola <amos@turnmill.co.za>; Anil Hegde <nottyanil@gmail.com>; antony jenis <antonyjenis@gmail.com>; Arun Jacob <jacob.igcs@gmail.com>; Arunachalam A <arunvani@gmail.com>; Ary Agung Prasetyo <ary_mt05@yahoo.com>; asad azmi <azmiasadayub@gmail.com>; Brl Pp <refazosaris@gmail.com>; Dindo <dindodelacruz@gmail.com>; Dinesh Somwanshi <som.din@gmail.com>; duc hoang <hoangvanduc79@gmail.com>; ENAYAT ZAREI <zarei.enayat@gmail.com>; Endri Prasetyo <endri.prasetyo@gmail.com>; Fitria Rahman <t.chintaqa@gmail.com>; fredric <fredric.prabu@bwgindia.com>; Garry Mat Eng. <garryirwin342@gmail.com>; Himan Nikdin <himannikdin@gmail.com>; james gerald <gerry_tup@yahoo.com>; John Henning <jhenning@deltak.com>; jose <joseseban@gmail.com>; Kaja Mohideen <kaja@asw.sa>; kannayeram gnanapandithan <kgpandithan@gmail.com>; Karthik <karthik6684@yahoo.com>; Kavin Murugam <kavin202082@yahoo.com>; ketan shah <ai.ketan@gmail.com>; khemici badri <khemicib@yahoo.fr>; lakshman kumar <lakshmankumar4@gmail.com>; Madhusudan Rout <madhusudan.rout@gmail.com>; mahesh sanghvi <sls.mahesh@gmail.com>; Mahmoud <mqreis@gmail.com>; materials-welding <materials-welding@googlegroups.com>; meemo prasad <meemoprasad@gmail.com>; Mehdi Emami <mehdi.emami@yahoo.com>; mpk mpk <ranmi2007@gmail.com>; MRG <mrgupta_2007@yahoo.com>; Muhammed Ibrahim PK <ibrat...@gmail.com>; muthu barathi <muthu_barathi@rediffmail.com>; "Nadgauda, Subhas" <subhas.nadgauda@jacobs.com>; Nandesh Kumar <nandeshkumar@rocketmail.com>; Narendra Gohil <ngohil@qafco.com.qa>; Neilash Kumar <neilashkumar@yahoo.com>; Nizam Mohamad <ahmad.nizam83@yahoo.com>; pgoswami <pgoswami@quickclic.net>; Pieper QSI <info@pieper-qsi.nl>; "prabhakarmet@gmail.com" <prabhakarmet@gmail.com>; prem nautiyal <prem_nautiyal26@yahoo.com>; R.Lenin <lenin8319@gmail.com>; rajeev arora <rajeevarora007@gmail.com>; rajkumarantoni <antonitr@gmail.com>; Ramchandra vichare <vicharerke@indiatimes.com>; Ramin Kondori <raminkondori@gmail.com>; ravi varman <ravimvarman@gmail.com>; S C Balawat <scb12345@gmail.com>; sanggyu LEE <sgleehong@gmail.com>; santhosh kumar <santhoshgu7@gmail.com>; SAQIB SHIRAZI <saqibshirazi83@hotmail.com>; sevak hiren <hirensevak80@gmail.com>; Shadab Alam Ansari <shadabansaria...@gmail.com>; shanmuga mari <85.ssmari@gmail.com>; snbagchi <snbagchi@aol.in>; Srinivas Engr <srinivas.gmsrini@gmail.com>; srinivasu <srinivasu.mech@gmail.com>; T. Mahendran <cbemahendar@yahoo.com>; U WYNN-NAING <u.wynn-naing@total.com>; vaibhav Joshi <vnjoshi.leo@gmail.com>; venkat ramana <venkatgps.ramana@gmail.com>; Vijay Katkar <katkar.vijay22@gmail.com>; vinit.deshpande <vinit.deshpande@akersolutions.com>; Vino Varghese <vinopvarghese@gmail.com>; Wu Hua <jointstars@yahoo.com>; yogeshkumar Kumbhar <kumbharyogeshv@gmail.com>; ZUL MAS <zulmas77@yahoo.com>
Sent: Wednesday, April 11, 2012 9:11 AM
Subject: Regarding Electrode Weaving

Respected Experts,


We generally mention in WPS/PQR weaving of Electrode should be three times the Electrode dia...I have query is Code restrict for this ,anywhere written in code aur it is on general experience...


Thanks & Regards
Mohit Aggarwal



--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...