Hi You can go for Equotip Portable hardness tester which is very reliable and costs @ 4 Lacs. Regards Prem Nautiyal --- On Fri, 3/16/12, pawan <pawan.tiwari@dwekam.org> wrote:
From: pawan <pawan.tiwari@dwekam.org> Subject: [MW:13897] best portable hardness tester-digital To: materials-welding@googlegroups.com Date: Friday, March 16, 2012, 5:49 PM
Pl. suggest best digital portable hardness tester (HRC) to check the weld metal hardness on 3layers pad. T&R Pawan tiwari -- To post to this group, send email to materials-welding@googlegroups.com To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com For more options, visit this group's bolg at http://materials-welding.blogspot.com/ The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
|
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/ The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.