Dear Mr. Manivannan,
Qualified welder of company 'B' can't weld any welding by using company 'A's WPS.
Instead, the company A could qualify company B's welder as per their (company A's) WPS to make welding of Company A's cast components.
T & R
R Vairamuthu
QA/QC Welding
Oman
From: hemumanivannan@gmail.com
Date: Fri, 16 Mar 2012 06:07:49 +0530
Subject: [MW:13891] Welder qualification
To: materials-welding@googlegroups.com
MANIVANNAN.P
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Qualified welder of company 'B' can't weld any welding by using company 'A's WPS.
Instead, the company A could qualify company B's welder as per their (company A's) WPS to make welding of Company A's cast components.
T & R
R Vairamuthu
QA/QC Welding
Oman
From: hemumanivannan@gmail.com
Date: Fri, 16 Mar 2012 06:07:49 +0530
Subject: [MW:13891] Welder qualification
To: materials-welding@googlegroups.com
Dear Experts,
Please clarify.
Situation: Company 'A' has given a subcontract to company 'B' for repair welding of cast components.
Company 'A'-holds qualified WPS as per ASME sec IX and issues copy of them to company 'B' to follow for his work.
Question: Can the vendor (company 'B') is permitted to make production weld by following WPS of company 'A' with company 'B's qualified welder? indicate code reference.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com