Tuesday, March 6, 2012

Re: [MW:13846] minimum distance limitation between two weld joints

Dear Murat,
Refer to your project specification its shall be mention some where,
but from my experience it shall be away from the heat effected zone of
the weld to avoid chance of metallurgical properties and best practice
is 2 x thickness of the base metal.
Correct me if I am wrong

On 3/6/12, murat aksoy <maksoy970@gmail.com> wrote:
> Hello my friends,
>
> I have a problem.
>
> Is there minimum distance limitation between two weld joints as per ASME
> B31.3. or EN
>
> thanks
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>


--
Best Regards

Mazlan Abd Aziz
Freelance Inspector
Email: mazlanaziz66@gmail.com
mazsp66@yahoo.com
Mobile:+6019-4772079

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...