Wednesday, February 8, 2012

Re: [MW:13637] What is meant by MGAL

Chaitanya,
May be this will help to some extent:


EN10025-2 allows the delivery conditions +M, +N or +AR at the manufacturers discretion.

FYI: None of these delivery conditions has any impact on the mechanical properties / chemical composition as defined in EN10025-2.

Delivery condition +MGAL is not defined in EN10025, it might be an internal manufacturer's code, e.g. +M, capable of forming a zinc layer during hot-dip galvanization.

Marc May | Senior Engineer
ArcelorMittal LCE Luxembourg / Commercial Sections S.A.


Best regards,

Shashank Vagal



--- On Wed, 8/2/12, Chaitanya Purohit <chaitanya_purohit@yahoo.co.in> wrote:

From: Chaitanya Purohit <chaitanya_purohit@yahoo.co.in>
Subject: [MW:13633] What is meant by MGAL
To: materials-welding@googlegroups.com
Date: Wednesday, 8 February, 2012, 12:07 PM

Dear All,

We have procured Flat bars of 60 x 40mm size with material specification S355 J2


In the MTC, material specification is S355 J2 + MGAL as per EN10025-2:2004

 

Can somebody, please clarify the meaning of 'MGAL' mentioned in MTC along with Material spec / Grade


 
C. K. Purohit
+968 92840112


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...