Re: [MW:13607] use ER316L to weld A312 TP 321

usaully SS 321 /310 materials used for high temperature service such as flare tips , Fired heater coils etc and you need to use ER 347 Ti /E 347 Ti consuambles
Frnacis
----- Original Message -----
From: Mumtaz Ali Khan <mumtaz.ali662000@gmail.com>
To: materials-welding@googlegroups.com
Sent: Thu, 2 Feb 2012 16:24:28 +0530 (IST)
Subject: Re: [MW:13604] use ER316L to weld A312 TP 321

ER347 for GTAW&E347 for SMAW process.316 will not work on such high temprature

On 2/2/12, Ramin Kondori <raminkondori@gmail.com> wrote:
> Normally 321 grade is being used because of its high temperature
> corrosion resistance and I do not think the designer has specified
> 321 just for fun...!!!
> By welding it with E316-L you won't have the same high temperature
> properties in weld area. because the weld metal will no longer be full
> austenitic and will fail at high temperatures.
>
> If that is not a problem then go ahead but I do not recommend that...!!!
>
> Regards
> Ramin Kondori
> IWE AT 0070
>
> On 2/2/12, Mohamed Elsayed ( BTG) <MElsayed@ccc.ae> wrote:
>> Gents,
>>
>> I need your valuable advice on following.
>>
>>
>>
>> We have some joints in for Flare package ,
>>
>>
>>
>> Can we use ER316L filler wire to weld
>>
>> 1- butt welded joints A312 TP 321
>>
>> 2- Butt welded Joints A403 WP 321
>>
>>
>>
>> Separatly ,
>>
>>
>>
>> We have supporting PQR USING ER316L welded material A240 316L , can
>> this PQR suppot welding
>>
>> 1- butt welded joints A312 TP 321
>>
>> 2- Butt welded Joints A403 WP 321
>>
>>
>>
>> Waitting your reply ASAP
>>
>>
>>
>> Thanks
>>
>> Mohamed
>>
>>
>>
>> --
>> To post to this group, send email to materials-welding@googlegroups.com
>> To unsubscribe from this group, send email to
>> materials-welding+unsubscribe@googlegroups.com
>> For more options, visit this group's bolg at
>> http://materials-welding.blogspot.com/
>> The views expressed/exchnaged in this group are members personel views and
>> meant for educational purposes only, Users must take their own decisions
>> w.r.t. applicable code/standard/contract documents.
>>
>
>
> --
> Ramin Kondori
> * QC/Welding Engineer *
> * IWE AT 0070*
>
>
> *با تشكر*
>
> * *
>
> *رامين كندري*
>
> واحد كنترل و تضمين كيفيت كارگاه ال ان جي كنگان
>
> شركت نارديس انرژي
>
> تلفن: 07727462189 داخلي 172 و171
>
> فكس: 07727462179
>
> همراه: 09132150320
>
> آدرس: كنگان - سايت LNG - دفتر شركت نارديس
>
> صندوق پستي 375 (اداره پست شهرستان كنگان)
>
>
>
> *Regards*
>
> *Ramin Kondori*
>
> QA/QC Manager
>
> IRAN-LNG Preoject
>
> NARDIS ENERGY CO.
>
> * *
>
> *Tel.: +98-772-7462189 (Int.171, 172)*
>
> *Fax: +98-772-7462179*
>
> *Cell: +98-913-215-0320*
>
> * Add.(Head office): No.27, 6th St., Seyed Jamalledin-e-Asad Abadi Ave.,
> Tehran, Iran, 1431784891*
> *Add.(Site): NARDIS Office, IRAN-LNG Plant, Kangan-Iran P.O.Box 375(Kangan
> Post Office) *
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35354] Cast-iron welding

1. Preheat joint area(other area, cover with mineral wool). 2. ENiCi or ENiFe-CI. 3. stringer bead. 4. peening is to be done on weldmetal im...