[MW:13653] Procedure qualification with Impact test & PWHT

Dear all,
 
Request your kind clarification on the below subject.
 
For Welding Procedure Qualification as per ASME SEC IX , with impact test and PWHT.
 
1) QW 407.2 states " The procedure qualification test shall be subjected to PWHT essentially equivalent to that encountered in the fabrication of production welds, including at least 80% of the aggregate times at temperature"
 
Question:
Can we use a PQR for a production weld,  which has PWHT to be done for a shorter duration than that recorded in the PQR. (e.g. PQR qualifed at 620 degC for 120minutes and production requirement 620 degC for 100 minutes)
 
2) Please find attached file.
 
regards
lsk
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...