Thursday, February 9, 2012

[MW:13639] Re: B-H curve of ASTM A 36

Mr.Hiren

Kindly let me know what is the BH Curve. And what purpose.

Regards

Santhosh

On Feb 8, 5:10 pm, sevak hiren <hirenseva...@gmail.com> wrote:
> Please find attached BH Curve for A36
>
> Regards
>
> Hiren Sevak
>
>
>
> On Fri, Feb 3, 2012 at 11:28 AM, hitesh patel <hitesh....@gmail.com> wrote:
> > Dear Experts
>
> > I  require the B-H curve for structural steel (ASTM A 36). Can any body
> > guide me for the same?
>
> > From where i could get this ?
>
> > Thanks
> > Hitesh Patel
>
> > --
> > To post to this group, send email to materials-welding@googlegroups.com
> > To unsubscribe from this group, send email to
> > materials-welding+unsubscribe@googlegroups.com
> > For more options, visit this group's bolg at
> >http://materials-welding.blogspot.com/
> > The views expressed/exchnaged in this group are members personel views and
> > meant for educational purposes only, Users must take their own decisions
> > w.r.t. applicable code/standard/contract documents.
>
> --
> Thanks & Regards
>
> Hiren Sevak
> Surveyor
> Bureau Veritas - Ahmedabad
> 207, Abhishree
> Opp Star India Bazaar,
> Satellite Road,
> Ahmedabad-380015
> Tel No. 079-26925491/92
>
>  BH Curve A 36.pdf
> 176KViewDownload

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...