Dear All,
-- We have procured Flat bars of 60 x 40mm size with material specification S355 J2
In the MTC, material specification is S355 J2 + MGAL as per EN10025-2:2004
Can somebody, please clarify the meaning of 'MGAL' mentioned in MTC along with Material spec / Grade
C. K. Purohit
+968 92840112
+968 92840112
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.