Wednesday, February 8, 2012

[MW:13629] RE: 13616] Welding 90Cu-10Ni to Carbon Steel.

Dear Sutthipong K.

The WPS with 90Cu+10Ni(P-No.34) weld to Carbonsteel(P-No.1);
By GTAW process you can try use wire ERNiCu-7 (N04060) ANSI/AWS A5.14

Regards
Ibnuziad

-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of LeONarD P
Sent: 06 Februari 2012 15:15
To: Materials & Welding
Subject: [MW:13616] Welding 90Cu-10Ni to Carbon Steel.

Dear Expert,

If I will qualified WPS with 90Cu+10Ni(P-No.34) weld to Carbon
steel(P-No.1);
By GTAW process. Can I choose the type of welding rod for
welding ? .Please reply
me in the light of ASME SEC IX.

Thanks in advance


Sutthipong K.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions
w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...