Could one give the interpretation clarity of the below :
1.Refer to ASME SEC.VIII .DIV.1 UCS-56 table for P9B materials under
note 3 (a) which states that qualification has to be done in equal or
greater thickness than the production weld thickness(Our customer
specs.(UDHE) also specifies that all welding procedures shall be
qualified on plates not thinner than the part to be welded.)
&
2.Refer to ASME SEC. IX QW-403.6 which states that minimum thickness
qualified is the thicknes of the test coupen or 16 mm whichever is
less .
While comparing the above 2 mentioned statement: Whether we need to
do the welding procedure qualification for each thickness with impact
& without PWHT?
Thanks,
kamal
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment