Re: [MW:11255] Heat Treatment information in MTC for ASTM A53B pipe

Yes, or arrive at some understanding with your client to take hardness and waive it
Or contact the manufacturer to get it included for re-issuing the MTC.
 
 
--- On Wed, 1/6/11, qaqcmpm <mamujeebali@gmail.com> wrote:

From: qaqcmpm <mamujeebali@gmail.com>
Subject: [MW:11234] Heat Treatment information in MTC for ASTM A53B pipe
To: "Materials & Welding" <materials-welding@googlegroups.com>
Date: Wednesday, 1 June, 2011, 7:19 PM

As per ASTM standard, ERW pipe (ASTM A53B) shall be heat treated above
540 deg c. But if the heat treatment information is not available in
the MTC, is it a Non conformance?

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...