Re: [MW:11230] RE: 11149] Re: Reduction temperature for LTCS

Q: if one welding joints two times came repair again one more repair
come then what will we do?

On 5/31/11, pgoswami <pgoswami@quickclic.net> wrote:
> Hello MPK,
>
> Please see the attached document ,which gives a broad overview of sour
> services both as per MR-0175(upstream) and MR-0103(downstream).Feel free ask
> more questions if you wish.
>
> Note:-to understand sour services one does not have to be a NACE Corrosion
> specialist. A person with good common sense and engineering background would
> be able to comprehend the requirements after reading through the above
> documents.
>
>
> Regarding " What is reduction temperature for LTCS" if you provide the
> details about the problem, I would be able to guide you.
>
> Thanks and best regards.
>
> Pradip Goswami,P.Eng.IWE
> Welding & Metallurgical Specialist & Consultant
> Ontario,Canada.
> Email-pgoswami@sympatico.ca,
> pgoswami@quickclic.net
>
> -----Original Message-----
> From: materials-welding@googlegroups.com
> [mailto:materials-welding@googlegroups.com] On Behalf Of Kannan
> Sent: Wednesday, May 25, 2011 12:26 PM
> To: Materials & Welding
> Subject: [MW:11149] Re: Reduction temperature for LTCS
>
> To understand Sour service you have to spend some time turning pages of NACE
> MR 0175 all parts and MR 0103 to start with. Later on API RPs.
> After that you are sure to become a corrosion specialist, depending on your
> understanding.
>
> I fail to understand your question "What is reduction temperature for LTCS
> ?"
>
> Kannan
>
> On May 18, 1:39 pm, mpk mpk <ranmi2...@gmail.com> wrote:
>> Dear Experts,
>>
>> What is reduction temperature for LTCS & what is sour service.
>>
>> Thank You.
>>
>> MPK..
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

Re: [MW:10788] ON PLOT PIPING & OFF PLOT PIPING

Piping systems involved for the flow lines and gathering lines from the well head isolation valve to the production facility or processing plant isolation valve are determined as OFF PLOT. ON PLOT defines piping system in the processing plant and production platform. ANSI/ASME B31.4 applies for off plot piping system. B31.4 allows the use of either API 1104 or ASME section IX (as appropriate). However, occasionally, a very small system such as piping within 500 feet of a processing plant (some client also said 400 feet) may be declared B31.3 rather than B31.4. When B31.3 is invoked, only ASME Section IX is used. before you decide which code to use for welding procedure and/or welder qualification for pipe welding, you have to know the design and construction code applicable to the system. Please read far enough into scope and diagram illustrating the application of either B31.3 and B31.4 hope this helps rgds 2011/4/21 pradip kumar sil < pradipsil@gmail.com > Dear all, ...