I THINK THE SOME HEAT TREATMENT ALSO CAN APPLY 100C TO ACHIEVE GOOD
WELDABILITY WITH NICKEL BASED ELECTRODE. ENI-1.
On May 30, 12:22 pm, we1414 <hamidhussain1...@yahoo.com> wrote:
> apply a surface layer on cast iron side with ENi-1 electrode ample
> enough to compensate dilution effects then weld it with any suitable
> welding electrode compatible with your carbon steel grade.
>
> On May 29, 4:29 pm, Ahmed Eissa <ahmedeiss...@yahoo.com> wrote:
>
>
>
>
>
>
>
> > dear experts
> >
> > does any one has welded carbon steel to cast iron before?
> > what filler metal to use?
> > what precausions should be taken?
> >
> > any valuable data will be appreciated.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments