Re: [MW:10751] visual test

am asking cumulative length of IP as per asme 31.3 normal  or M service .

On Tue, Apr 19, 2011 at 4:26 PM, Jean Staton <Jean.Staton@metco-ndt.com> wrote:

B31.3 Severe does not allow I.P however Normal allows 1 ½" in 6" (38mm in any 150 mm of weld length) be careful of what code you are responding to.

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Fitria Rahman
Sent: Monday, April 18, 2011 7:06 PM

Subject: Re: [MW:10725] visual test

 

Dear Senthil

If your code is B31.3, please refer to table 341.3.2 to get the answer. Incomplete penetration and surface porosity are not acceptable (no imperfection).

rgds

2011/4/18 SENTHIL P <senbe381@gmail.com>

Dear sir,
      6 "  std pipe 7.11mm for normal and M fluid
visually we find incomplete pentration 34mm in any 150mm ,depth 2mm in random manner, is it accepted? please explain
 and we find 1mm or small visually seen porosity on surface of weld ,is need to repair or not? we can grind this but prodution  people not allowed, please explain
 thank u,
senthil

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



DISCLAIMER: The information contained in this e-mail may be confidential and is intended solely for the use of the named addressee. Access, copying or re-use of the e-mail or any information contained therein by any other person is not authorized. If you are not the intended recipient please notify us immediately by returning the e-mail to the originator.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...