Tuesday, April 5, 2011

Re: [MW:10605] Weaving

Kindly check ASME II part C , A 6.1.4

--- On Tue, 4/5/11, Ahmed Husain <ahmraha@yahoo.com> wrote:

From: Ahmed Husain <ahmraha@yahoo.com>
Subject: Re: [MW:10597] Weaving
To: materials-welding@googlegroups.com
Date: Tuesday, April 5, 2011, 7:42 AM

Dear All,
 
Almost all SMAW WPS prepared in accordance to ASME IX, I have seen, it specify maximum weaving 3 times the electrode dia. But I am unable to co-relate this WPS requirement to any ASME code or Client (ARAMCO) requirement . If weaving 3 times electrode dia is not stated in ASME codes, then why does it is mentioned in WPS?
 
Kindly share some information on this subject.
 

 
Ahmed Husain
Mob-0547170325



From: ramu ramalingam <ramu.srivi@gmail.com>
To: materials-welding@googlegroups.com
Sent: Fri, April 1, 2011 9:49:05 AM
Subject: Re: [MW:10554] Weaving

Hai,
 
If they want to weave more than 3 times of electrode/filler wire dia, better to make new WPS and proof all the necessary requirement to meet with old WPS.
 
Because,when we weave more, in production weld that time heat input will be increased and  its fail in tenstile test. The heat inputput  should not be more than 3 KJ/min for each process.

Regards,
RR
 
On Wed, Mar 23, 2011 at 11:31 PM, Sampath Kumar <skthatham@gmail.com> wrote:
Dear Friends,
 
WPS says the weaving is allowed/permitted 3times the diameter of the electrode.Please tell me wheather we can allow if the weaving is more than the allowable limit.If it can be allowed.What is the reasons and on what basis it is allowed?If it can not/should not be allowed.Why and what is the reasons?
 
My opinion is that it should not be allowed.[1]Because it deviates from the WPS.[2]properties may vary because of the excess heat In put due to excess weaving.
 
The contractor is of opinion that they will change the WPS to suit excess weaving.It is not an essential variable,hence it can be allowed.To substantiate their claim they say they will change the WPS and they will perform Hardness Test to prove that the properties were not changed.
With Best Regards
Sampath
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...