Monday, February 14, 2011

Re: [MW:9870] I.Q.I

Dear Mr.Ali,
the attached document may help you ,
please refer EN 462-1 Image quality of Radiographs (IQI)


--
Thanks & Regards.

Santosh Gaikwad

Material Testing & Inspection Services(MTIS),
Surat,India.



On Mon, Feb 14, 2011 at 5:46 AM, ali asghari <asgharialigl@gmail.com> wrote:
Dear All
 for radiography of duplex stainless steel ,the material of I.Q.I must be from this type or not according to ASME sec V?
Grouping of material in SE747 only mention to Carbon steel and seri 300 stainless steel.
regards

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...