Re: [MW:9867] I.Q.I

Gen,
 
All of this requirements should be mention on procedure.
Here I use ASTM group A for low pressure and FE EN vice versa
 
 
Leo
 
 

--- On Mon, 2/14/11, ali asghari <asgharialigl@gmail.com> wrote:

From: ali asghari <asgharialigl@gmail.com>
Subject: [MW:9856] I.Q.I
To: materials-welding@googlegroups.com
Date: Monday, February 14, 2011, 11:46 AM

Dear All
 for radiography of duplex stainless steel ,the material of I.Q.I must be from this type or not according to ASME sec V?
Grouping of material in SE747 only mention to Carbon steel and seri 300 stainless steel.
regards
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...