Re: [MW:9825] Hot-tap hole

Hi.
If you instaling a split tee with welding this should not be permitted closer than

18 in. (46 cm) to a flange or threaded connection, or approxi-

Mately 3 in. (8 cm) to a welded seam (including a longitudi-

nal seam of welded piping)

 
Agustin




De: Eduardo Calva <eduardocalva@hotmail.com>
Para: materials-welding@googlegroups.com
Enviado: jue, febrero 10, 2011 9:34:45 PM
Asunto: [MW:9805] Hot-tap hole

Dears, could you please tell me what this statement of API RP-2201 mean?

 

6.8 WELDING AND HOT TAP CONNECTION DESIGN

Welding or hot tapping should not be permitted closer than

18 in. (46 cm) to a flange or threaded connection, or approxi-

Mately 3 in. (8 cm) to a welded seam (including a longitudi-

nal seam of welded piping) unless determined by an

engineering review to be acceptable.

 

 

Eduardo Calva


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...