Re: [MW:9815] ASME Sec. VIII Div. 1 - MDR form U1 / U1A

You put your address but there is also place to put the clients address
Best regards
Dr Georgios Dilintas
Authorized Nuclear Inspector
Authorized Inspector Supervisor
HBS Regional Technical Manager


----- Original Message -----
From: Prasad [prsgne@gmail.com]
Sent: 10/02/2011 21:08 PST
To: "Materials & Welding" <materials-welding@googlegroups.com>
Subject: [MW:9813] ASME Sec. VIII Div. 1 - MDR form U1 / U1A

Dear experts & ASME Authorized Inspectors,


Our company have ASME certificate of authorization for ASME U stamp
with scop covering
manufacturing activities at shop & field sites controlled by our
company.
We have constructed a pressure vessel at field site owened by our
customer.
Now we have to prepare MDR in U1 form.
My question is againest name & address of manufacturer whether we have
to put field site address or address of our company as apeared on
certificate of authorization.

Please share your experience & views on above.

Thanking you.

Prasad

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...