Re: [MW:9794] special requierment in NACE electrode

Dear James,
thanks for your grate support,
I want to know for both NACE MR 0175 & NACE MR 0103.
base material is carbonsteel P NO:1
regards

On Tue, Feb 8, 2011 at 9:39 PM, james gerald <gerry_tup@yahoo.com> wrote:
> Viral,
>
> Please specify whether it is for upstream(NACE MR0175) or for Refinery(NACE MR0103). Specify for which Base materials the welding need to be performed.
>
> J.GERALD JAYAKUMAR  00919344954677
>
>
> --- On Tue, 2/8/11, viral talati <viraltalati.143@gmail.com> wrote:
>
>> From: viral talati <viraltalati.143@gmail.com>
>> Subject: [MW:9786] special requierment in NACE electrode
>> To: materials-welding@googlegroups.com
>> Date: Tuesday, February 8, 2011, 5:11 PM
>> Dear Friends,
>> Is there any special requierment for electrode used for
>> NACE material welding.
>>
>> regards
>>
>> --
>> To post to this group, send email to materials-welding@googlegroups.com
>> To unsubscribe from this group, send email to
>> materials-welding+unsubscribe@googlegroups.com
>> For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>> The views expressed/exchnaged in this group are members
>> personel views and meant for educational purposes only,
>> Users must take their own decisions w.r.t. applicable
>> code/standard/contract documents.
>>
>
>
>
> ____________________________________________________________________________________
> No need to miss a message. Get email on-the-go
> with Yahoo! Mail for Mobile. Get started.
> http://mobile.yahoo.com/mail
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...