Re: [MW:9784] Having GTAW, 6G, 8"Dia 5 to 25.4mm WPS, 2" welder qualification posible or not? as per ASME Sec 9

I think 452.3 can not apply to WPS as 452.3 is for performance qualification and not procedure qualification.

I think WPS is qualified for all diameters as per section ix and for welder qualified with above wps by welding 2'' pipe, his qualification range (diameters )will be governed by 452.3

On Tue, Feb 8, 2011 at 9:20 AM, Engineer Mech <mengineer010@gmail.com> wrote:
Dear All

I am having GTAW  6G wps.
PQR dia is 8"
Thk: 5 to 25.4mm
My question is.  With above WPS can i qualify welder in 2" Dia test
Piece?
either we have to consider  452.3 diameter limits.?

Tnks

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...