           Thanks for your valuable inputs. My vessel was constructed as per sec VIII Div 1 and its service was sea water with rubber lined. We had internal corrosion underneath the lining where outlet piping located and due to this there was leak reported.
 
So we have given to our contractor to have complete repair by welding and relining rubber coating of the vessel. Now it seems the repair works completed and I have to inspect and accept it.
 
       Could you explain me that what are things should I check prior to my acceptance of the vessel?
 
Thank you,
Ilan

--- On Mon, 2/7/11, muthu barathi <muthu_barathi@rediffmail.com> wrote:

From: muthu barathi <muthu_barathi@rediffmail.com>
Subject: Re: [MW:9757] sea water filter
To: materials-welding@googlegroups.com
Date: Monday, February 7, 2011, 5:01 PM

Hi,

You have not mentioned which code it is constructed. what type of
repair is carried out any weld took place if any welding then u have
to go for hydrostatic test. secondly you have to go for holiday test
for your rubber lining visual . if all ok u can accept the vessel.



On Mon, 07 Feb 2011 09:23:36 +0530 wrote
>Dear experts, We have found internal corrosion beneath the rubber
lining of sea water filter vessel. Now repair works is completed as per
our contractor. Could you please furnish me what should I check prior
to accept my vessel? The vessel made with carbon steel and the rubber
lining 5mm lined internally to avoid corrosion. I need your valuable
inputs if possible some notes.Thank you,Ilan
**********************************************************************B
orouge is a leading provider of value creating, innovative plastics
solutions for customers in the Middle East, Asia-Pacific and Africa.
Borouge employs unique Borstar® technology to produce differentiated
products for high-value infrastructure applications, including water,
gas and industrial pipe systems, power and communication cables,
advanced packaging and automotive components. Borouge's state-of-the-
art petrochemical complex is located at Ruwais, Abu Dhabi in the United
Arab Emirates.
=======================================================================
============
>CONFIDENTIALITY NOTICEThis email and any files transmitted with it are
confidential and intended solely for the use of the individual or
entity to whom they are addressed. If you have received this email in
error please delete the email and any attachment(s) and notify the
sender.This footnote also confirms that this email message has been
scanned for the presence of computer viruses.
>======================================================================
======================================= 




--
>
To post to this group, send email to materials-welding@googlegroups.com
>
To unsubscribe from this group, send email to materials-
welding+unsubscribe@googlegroups.com
>
For more options, visit this group's bolg at http://materials-
welding.blogspot.com/
>
The views expressed/exchnaged in this group are members personel views
and meant for educational purposes only, Users must take their own
decisions w.r.t. applicable code/standard/contract documents.
>


Dear Sir,





Thanking You,

Honesty is the best Policy

With Warm Regards,

Muthu Barathi P
Mobile No:00962788269821 (Jordan)
00962775401951
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...