Re: [MW:9711] Welding on top of a weld


In this case try to rotate or flush grind the butt weld and carry out
RT or UT of weld and if the weld is sound then carry out fillet weld it
is acceptable

On Thu, 03 Feb 2011 15:42:15 +0530 wrote
>Hello,

I have a case where the edge of the saddle of a pipe support coincides
with the pipe's butt weld. Code is B31.1-2007. The edge is supposed to
be fillet welded onto the pipe.
Is this permissible?


Thanks

Johnson




--
>
To post to this group, send email to materials-welding@googlegroups.com
>
To unsubscribe from this group, send email to materials-
welding+unsubscribe@googlegroups.com
>
For more options, visit this group's bolg at http://materials-
welding.blogspot.com/
>
The views expressed/exchnaged in this group are members personel views
and meant for educational purposes only, Users must take their own
decisions w.r.t. applicable code/standard/contract documents.
>


Dear Sir,





Thanking You,

Honesty is the best Policy

With Warm Regards,

Muthu Barathi P
Mobile No:00962788269821 (Jordan)
00962775401951

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate