Hi Karthik,
so you mean to say IS 2062 grade C is same as ABS AH36 Gr A.
rgds,
chakri
On Wed, Feb 2, 2011 at 11:27 AM, Karthik <karthik6684@yahoo.com> wrote:
http://www.splav.kharkov.com/steelgrade/mat_start_eu.php?name_id=10#1
or
http://www.arcelormittal.com/fce/prd_web/new_web_details.pl?code=A30&langlist=EN
Equivalent grades of grade S355J2 (1.0577)
USA
-Germany
DIN,WNrJapan
JISEuropean old
ENChina
GBSweden
SS
A656
St52-3N
SS490YA
Fe510D2 S355J2G4
Q345D
2134-01
Thanks & Regards,(Karthik)Karthikeyan.SQA/QC ManagerGetabec Energy Co.,Ltd.379,Moo6,Soi8,Nikhomphatana,Rayong-21180,Thailand.Phone: 0066 38 897035-8 (Off)Fax: 0066 38 897034Hand Phone: 0066 892512282
--- On Wed, 2/2/11, bujji <chakri.cruise@gmail.com> wrote:
From: bujji <chakri.cruise@gmail.com>
Subject: [MW:9676] details of equivalent materials list
To: materials-welding@googlegroups.com
Date: Wednesday, February 2, 2011, 2:51 PM
--Hi All,can anyone give me the details of equivalent materials list ?For eg : S355k2+N is EH-36 (40 MM plates)S355 J2 is equivalent to ----------- ??? (round bar dia 70 mm)Regards,chakri.
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment