Dear Muthu,


Please let me know....Which standard you are refered

Noushad

On 2/2/11, muthu barathi <muthu_barathi@rediffmail.com> wrote:
> Hi,
>
> It + /-5 degree C or 2% whichever is less.
>
>
> On Wed, 02 Feb 2011 10:59:52 +0530 wrote
>>Hello good morning,
>
>
>
> I need details of electrode oven calibration.
>
>
>
> How much percentage of temeparature variotion is allowable for
>
> electrode oven calibration
>
>
>
> --
>
> To post to this group, send email to materials-welding@googlegroups.com
>
> To unsubscribe from this group, send email to materials-
> welding+unsubscribe@googlegroups.com
>
> For more options, visit this group's bolg at http://materials-
> welding.blogspot.com/
>
> The views expressed/exchnaged in this group are members personel views
> and meant for educational purposes only, Users must take their own
> decisions w.r.t. applicable code/standard/contract documents.
>
>
>
> Dear Sir,
>
>
>
>
>
> Thanking You,
>
> Honesty is the best Policy
>
> With Warm Regards,
>
> Muthu Barathi P
> Mobile No:00962788269821 (Jordan)
> 00962775401951
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...