[MW:9833] RE: 9821] SA 516 Gr.60 high in manganese-accept or reject

For SA 516 Gr. 60 upto ½” thickness the manganese should be 0.6 to 0.9.

 

With kind regards,

Vinod Kumar Kataria

GM - Operations

Bliss Anand Private Limited,

92B/93B Sector 5

IMT Manesar,Gurgaon,

National Capital Region Delhi.

India .

Phone : +91-124-4366000 (9 Lines)

Mobile Phone : +91-9560199004

Fax : +91-124-2290884

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of krishna
Sent: Friday, February 11, 2011 5:02 PM
To: materialswelding
Subject: [MW:9821] SA 516 Gr.60 high in manganese-accept or reject

 

Dear all,
                  We have received MTC for SA 516 Gr.60 plate of 10mm thickness with manganese of 1.47%,the lab test also give the same.

is it acceptable as per SA 516 SPEC.

Please confirm shall we accept or reject the plates,we have procured more tonnes of materails & started fabrication?

what shall we do in this stage?

How to overcome this issue ,pls guide

krishna


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...