Friday, February 11, 2011

[MW:9827] RE: 9813] ASME Sec. VIII Div. 1 - MDR form U1 / U1A

I was not sure my response went through this morning, so here it is
again.
You use the information on your authorized certificates. Address,
company name, certificate registration number.

-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of Prasad
Sent: Thursday, February 10, 2011 11:09 PM
To: Materials & Welding
Subject: [MW:9813] ASME Sec. VIII Div. 1 - MDR form U1 / U1A

Dear experts & ASME Authorized Inspectors,


Our company have ASME certificate of authorization for ASME U stamp
with scop covering
manufacturing activities at shop & field sites controlled by our
company.
We have constructed a pressure vessel at field site owened by our
customer.
Now we have to prepare MDR in U1 form.
My question is againest name & address of manufacturer whether we have
to put field site address or address of our company as apeared on
certificate of authorization.

Please share your experience & views on above.

Thanking you.

Prasad

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views
and meant for educational purposes only, Users must take their own
decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...