Friday, February 11, 2011

[MW:9816] HIC test as per NACE MR 0103 of SA 516 Gr.60 plates

hi all,
        pls guide in the below query
 
we have to do a heat exchanger of material SA 516 Gr,60 conforming to NACE MR 0103.
 
we have ordered  for plates supply to a trader and do check test to conform the requirements of NACE MR 0103
 
what are all the test to be done as per NACE MR 0103?
 
Whether we have go for HIC test or not?
 
If we have to do HIC test for plate materails as per NACE where the clause is mentioned?
 
I have gone through NACE MR 0103 and could not interpret exactly whether HIC test is mandatory
 
please put all your comments related to this
 
kamal

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...