[MW:9739] Grouping of steels

Dear Friends,

Please let me know Grouping of Steels.Material is API 5 L Grade X 65.
This material falls under which group as per BS EN 288-3. My scenario is,
my material is API 5L grade X 65, I have to follow BS EN 288-3 for
welding procedure qualification and welders will be qualified as per BS
EN 287-1. For both welder qualification and and procedure qualification
the code shall be followed AWS D 1.1 - 2010.

Please give me your valuable suggestions.



Dear Sir,





Thanking You,

Honesty is the best Policy

With Warm Regards,

Muthu Barathi P
Mobile No:00962788269821 (Jordan)
00962775401951

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...