Friday, February 4, 2011

[MW:9727] PWHT Requirement

Dear Experts
 
Kindly share your expertise on the following question..
We are qualifying a WPS (SA 106Gr.B) with PWHT requirement so question is that what should be the timing gap to start PWHT after welding.
(Applicable : Sec.IX,ASME B31.3,ASTM D1.1)
Kindly mention code clause for reference.

Best Regards

Sandesh Pandey

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...